| Use the Perfection
chamfering tool for a proper O.D. chamfer. This chamfer
permits the PE piping to be completely stabbed without
affecting the internal seals. |
|
|
| Use a soft felt tip
pen, crayon or grease pencil to mark the stab depth
as indicated on your Hydrosert package instructions.
The stab depth is the approximate distance from the
edge of the fusion bead to the end of the fitting body. |
|
|
Stab the PE piping
into the hydrosert fitting so that the stab depth mark
is visible:
Within 1/8" of moisture seal on 1" CTS
sizes
Within 1/4" on all other sizes
The PE piping must bottom out in the fitting. Pressure
test the joint in accordance with your standard procedures.
The reference mark can move outward up to an additional
3/8" during pressure testing. |
|